Refractory for electric arc furnace lid

EAF uses A1203 65% -85% alumina brick masonry lid, the special needs of the site is also used tabular alumina brick (with a plate Al20390% -100%), but the price is expensive, silica brick is about 10 times higher 31V or thermal stress relief lid damaging effects of aluminum bricks, high alumina brick firing using phosphate bonded alumina bricks do not burn with white masonry made good use of effects. Some (HP) in high power electric furnace cover, the main use of high alumina bricks (about 80% Al2 03) and chemically bonded magnesia-chrome brick (Mg0> 65%, Cr2 037% _15%) Consolidated masonry furnace cover. High power (UHP) electric cover using mullite corundum brick, the brick main feature is a good thermal stability, resistance to high temperature load-deformation ability, it just to meet the requirements of the lid refractories, MK-80, No. MO corundum bricks,
is fused corundum and fused mullite particles strengthen the structure of products. 50t UHP EAF for cover, stainless steel and bearing steel smelting life increased by 25% -35% higher than magnesia-chrome brick roof.


High alumina brick lid. Alumina brick masonry furnace lid began in the late 1950s. At that time the use of high alumina brick lid (Ak 0365% -80%) increased by 4 times higher than silica brick lid life. Firing alumina bricks (A \ 2 03 80 16) and phosphate binding does not burn alumina brick (Al2 03 80% -85%) and mullite brick firing or not firing phosphate binding mullite brick, they have in common is an excellent thermal shock resistance. The life of the early 1960s, the lid has reached about 200 furnaces.

没有评论:

发表评论